{"id":90,"date":"2022-02-17T23:22:38","date_gmt":"2022-02-17T20:22:38","guid":{"rendered":"https:\/\/www.petroluber.com\/tr_TR\/?p=90"},"modified":"2022-04-20T17:12:11","modified_gmt":"2022-04-20T14:12:11","slug":"petroluber-h-11-kone-yagi","status":"publish","type":"post","link":"https:\/\/www.petroluber.com\/tr_TR\/petroluber-h-11-kone-yagi.html","title":{"rendered":"H-11 Kone Ya\u011f\u0131"},"content":{"rendered":"\n<div class=\"wp-block-safirtema-mainheading mainHeading\"><div class=\"icon icon6\"><\/div><div class=\"text\">Kone Ya\u011f\u0131<\/div><\/div>\n\n\n\n<p>Petroluber H-11 kone ya\u011f\u0131 , Y\u00fcksek h\u0131zl\u0131 makinelerde tekst\u00fcre polyester ya\u011flamas\u0131nda anti-splash \u00f6zellikli, polyester iplikler i\u00e7in mineral bazl\u0131 kone ya\u011f\u0131, iplik\/metal ve iplik\/iplik s\u00fcrt\u00fcnmelerini d\u00fc\u015f\u00fcr\u00fcr. Y\u00fcksek seviye anti-statik koruma sa\u011flar. Geleneksel y\u0131kama prosesi yeterlidir.<\/p>\n\n\n\n<div class=\"wp-block-safirtema-mainheading mainHeading\"><div class=\"icon icon55\"><\/div><div class=\"text\">Tipik Fiziksel ve Kimyasal Karakteristi\u011fi<\/div><\/div>\n\n\n\n<figure class=\"wp-block-table is-style-regular\"><table><tbody><tr><td class=\"has-text-align-center\" data-align=\"center\"><strong>K. Viskozite 40\u00b0C [mm\u00b2\/s]<\/strong><br><em>(ASTM D 445)<\/em><\/td><td class=\"has-text-align-center\" data-align=\"center\"><strong>K. Viskozite 100\u00b0C [mm\u00b2\/s]<\/strong><br><em>(ASTM D 445)<\/em><\/td><td class=\"has-text-align-center\" data-align=\"center\"><strong><strong>Parlama Noktas\u0131 [\u00b0C]<\/strong><br><\/strong><em>(ASTM D 92)<\/em><\/td><td class=\"has-text-align-center\" data-align=\"center\"><strong>Akma Noktas\u0131 [\u00b0C]<\/strong><br><em>(ASTM D 97)<\/em><\/td><\/tr><tr><td class=\"has-text-align-center\" data-align=\"center\">15<\/td><td class=\"has-text-align-center\" data-align=\"center\">3,2<\/td><td class=\"has-text-align-center\" data-align=\"center\">95<\/td><td class=\"has-text-align-center\" data-align=\"center\">178<\/td><\/tr><tr><td class=\"has-text-align-center\" data-align=\"center\">22<\/td><td class=\"has-text-align-center\" data-align=\"center\">3,9<\/td><td class=\"has-text-align-center\" data-align=\"center\">95<\/td><td class=\"has-text-align-center\" data-align=\"center\">186<\/td><\/tr><tr><td class=\"has-text-align-center\" data-align=\"center\">32<\/td><td class=\"has-text-align-center\" data-align=\"center\">5,2<\/td><td class=\"has-text-align-center\" data-align=\"center\">95<\/td><td class=\"has-text-align-center\" data-align=\"center\">194<\/td><\/tr><tr><td class=\"has-text-align-center\" data-align=\"center\">46<\/td><td class=\"has-text-align-center\" data-align=\"center\">6,5<\/td><td class=\"has-text-align-center\" data-align=\"center\">95<\/td><td class=\"has-text-align-center\" data-align=\"center\">228<\/td><\/tr><\/tbody><\/table><\/figure>\n","protected":false},"excerpt":{"rendered":"<p>Petroluber H-11 kone ya\u011f\u0131 , Y\u00fcksek h\u0131zl\u0131 makinelerde tekst\u00fcre polyester ya\u011flamas\u0131nda anti-splash \u00f6zellikli, polyester iplikler i\u00e7in mineral bazl\u0131 kone ya\u011f\u0131, iplik\/metal ve iplik\/iplik s\u00fcrt\u00fcnmelerini d\u00fc\u015f\u00fcr\u00fcr. Y\u00fcksek seviye anti-statik koruma sa\u011flar. Geleneksel y\u0131kama prosesi yeterlidir. K. Viskozite 40\u00b0C [mm\u00b2\/s](ASTM D 445) K. Viskozite 100\u00b0C [mm\u00b2\/s](ASTM D 445) Parlama Noktas\u0131 [\u00b0C](ASTM D 92) Akma Noktas\u0131 [\u00b0C](ASTM D [&hellip;]<\/p>\n","protected":false},"author":1,"featured_media":1352,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":[],"categories":[7,19],"tags":[20,127,192],"_links":{"self":[{"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/posts\/90"}],"collection":[{"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/comments?post=90"}],"version-history":[{"count":4,"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/posts\/90\/revisions"}],"predecessor-version":[{"id":2049,"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/posts\/90\/revisions\/2049"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/media\/1352"}],"wp:attachment":[{"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/media?parent=90"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/categories?post=90"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/www.petroluber.com\/tr_TR\/wp-json\/wp\/v2\/tags?post=90"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}